佳 盼 塑 胶
JIA PAN SU JIAO
/ Product details
/ classification
LNP™ THERMOCOMP™ PBT WH0270F compound
聚丁烯对苯二甲酸酯
专有填料
SABIC Innovative Plastics
产品说明
LNP* THERMOCOMP* WH0270F is a compound based on PBT resin containing Proprietary Filler(s). Added feature of this material is: High Specific Gravity.
Also known as: LNP* THERMOCOMP* Compound WH0270FX
Product reorder name: WH0270F
填料增强:含专有填料
材料特点:高比重
塑料牌号:PBT WH0270F compound
加工方法:注射成型
定属记号:PBT
材料物性
物理性能 |
额定值 |
单位制 |
测试方法 |
密度 |
2.70 |
g/cm³ |
ASTM D792 |
收缩率 |
|
|
ASTM D955 |
流动:24小时 |
1.1 |
% |
|
横向流动:24小时 |
1.3 |
% |
|
吸水率(24 hr,50% RH) |
0.080 |
% |
ASTM D570 |
机械性能 |
额定值 |
单位制 |
测试方法 |
拉伸模量 |
|
|
|
--2 |
10500 |
MPa |
ASTM D638 |
-- |
8290 |
MPa |
ISO 527-2/1 |
抗张强度 |
|
|
|
屈服3 |
31.9 |
MPa |
ASTM D638 |
屈服 |
31.5 |
MPa |
ISO 527-2/5 |
断裂3 |
31.4 |
MPa |
ASTM D638 |
断裂 |
31.0 |
MPa |
ISO 527-2/5 |
伸长率 |
|
|
|
屈服3 |
0.58 |
% |
ASTM D638 |
屈服 |
0.57 |
% |
ISO 527-2/5 |
断裂3 |
0.74 |
% |
ASTM D638 |
断裂 |
0.72 |
% |
ISO 527-2/5 |
弯曲模量 |
|
|
|
50.0 mm 跨距4 |
8330 |
MPa |
ASTM D790 |
--5 |
8320 |
MPa |
ISO 178 |
弯曲强度 |
|
|
|
--5,6 |
52.3 |
MPa |
ISO 178 |
屈服,50.0 mm 跨距4 |
56.3 |
MPa |
ASTM D790 |
断裂抗挠强度7 |
0.83 |
% |
ISO 178 |
冲击性能 |
额定值 |
单位制 |
测试方法 |
悬壁梁缺口冲击强度 |
|
|
|
23℃ |
19 |
J/m |
ASTM D256 |
23℃8 |
3.4 |
kJ/m² |
ISO 180/1A |
无缺口悬臂梁冲击 |
|
|
|
23℃ |
150 |
J/m |
ASTM D4812 |
23℃8 |
11 |
kJ/m² |
ISO 180/1U |
装有测量仪表的落镖冲击(23℃,Total Energy) |
3.92 |
J |
ASTM D3763 |
热性能 |
额定值 |
单位制 |
测试方法 |
热变形温度 |
|
|
|
1.8 MPa,未退火,3.20 mm |
164 |
℃ |
ASTM D648 |
1.8 MPa,未退火,64.0 mm 跨距9 |
162 |
℃ |
ISO 75-2/Af |
线形膨胀系数 |
|
|
ASTM E831 |
流动:-30 到 30℃ |
0.000043到0.000045 |
cm/cm/℃ |
|
横向:-30 到 30℃ |
0.000058到0.000060 |
cm/cm/℃ |
|
注射 |
额定值 |
单位制 |
|
干燥温度 |
121 |
℃ |
|
干燥时间 |
4.0 |
hr |
|
建议的最大水分含量 |
0.050 |
% |
|
螺筒后部温度 |
221 到 232 |
℃ |
|
螺筒中部温度 |
243 到 254 |
℃ |
|
螺筒前部温度 |
260 到 271 |
℃ |
|
加工(熔体)温度 |
238 到 266 |
℃ |
|
模具温度 |
82.2 到 98.9 |
℃ |
|
背压 |
0.172 到 0.344 |
MPa |
|
螺杆转速 |
30 到 60 |
rpm |