佳 盼 塑 胶
JIA PAN SU JIAO
/ Product details
/ classification


LNP™ THERMOTUF™ PA6 PX95726 compound
聚酰胺6
玻璃纤维增强材料
SABIC Innovative Plastics
产品说明
LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Also known as: LNP* THERMOTUF* Compound PDX-P-95726
Product reorder name: PX95726
填料增强:含玻璃纤维增强
含添加剂:热稳定剂
材料特点:热稳定
塑料牌号:PA6 PX95726
定属记号:尼龙6
加工方法:注射成型
	
材料物性
| 
				 物理性能  | 
			
				 额定值  | 
			
				 单位制  | 
			
				 测试方法  | 
		
| 
				 比重  | 
			
				 1.22  | 
			
				 g/cm³  | 
			
				 ASTM D792  | 
		
| 
				 收缩率  | 
			
				 | 
			
				 | 
			
				 ASTM D955  | 
		
| 
				 流动:24小时  | 
			
				 0.30 到 0.60  | 
			
				 %  | 
		|
| 
				 横向流动:24小时  | 
			
				 0.80 到 1.1  | 
			
				 %  | 
		|
| 
				 吸水率  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 24 hr,50% RH  | 
			
				 1.1  | 
			
				 %  | 
			
				 ASTM D570  | 
		
| 
				 平衡,23℃,50% RH  | 
			
				 1.6  | 
			
				 %  | 
			
				 ISO 62  | 
		
| 
				 机械性能  | 
			
				 额定值  | 
			
				 单位制  | 
			
				 测试方法  | 
		
| 
				 拉伸模量  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 --2  | 
			
				 5840  | 
			
				 MPa  | 
			
				 ASTM D638  | 
		
| 
				 --  | 
			
				 5800  | 
			
				 MPa  | 
			
				 ISO 527-2/1  | 
		
| 
				 抗张强度  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 屈服3  | 
			
				 111  | 
			
				 MPa  | 
			
				 ASTM D638  | 
		
| 
				 屈服  | 
			
				 109  | 
			
				 MPa  | 
			
				 ISO 527-2/5  | 
		
| 
				 断裂  | 
			
				 107  | 
			
				 MPa  | 
			
				 ASTM D638  | 
		
| 
				 断裂3  | 
			
				 108  | 
			
				 MPa  | 
			
				 ASTM D638  | 
		
| 
				 断裂  | 
			
				 105  | 
			
				 MPa  | 
			
				 ISO 527-2/5  | 
		
| 
				 伸长率  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 屈服3  | 
			
				 3.1  | 
			
				 %  | 
			
				 ASTM D638  | 
		
| 
				 屈服  | 
			
				 3.1  | 
			
				 %  | 
			
				 ISO 527-2/5  | 
		
| 
				 断裂3  | 
			
				 3.7  | 
			
				 %  | 
			
				 ASTM D638  | 
		
| 
				 断裂  | 
			
				 3.8  | 
			
				 %  | 
			
				 ISO 527-2/5  | 
		
| 
				 弯曲模量  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 --  | 
			
				 5030  | 
			
				 MPa  | 
			
				 ASTM D790  | 
		
| 
				 50.0 mm 跨距4  | 
			
				 4960  | 
			
				 MPa  | 
			
				 ASTM D790  | 
		
| 
				 --5  | 
			
				 4790  | 
			
				 MPa  | 
			
				 ISO 178  | 
		
| 
				 弯曲强度  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 --  | 
			
				 171  | 
			
				 MPa  | 
			
				 ASTM D790  | 
		
| 
				 --  | 
			
				 160  | 
			
				 MPa  | 
			
				 ISO 178  | 
		
| 
				 屈服,50.0 mm 跨距4  | 
			
				 173  | 
			
				 MPa  | 
			
				 ASTM D790  | 
		
| 
				 冲击性能  | 
			
				 额定值  | 
			
				 单位制  | 
			
				 测试方法  | 
		
| 
				 悬壁梁缺口冲击强度  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 23℃  | 
			
				 68  | 
			
				 J/m  | 
			
				 ASTM D256  | 
		
| 
				 23℃6  | 
			
				 6.7  | 
			
				 kJ/m²  | 
			
				 ISO 180/1A  | 
		
| 
				 无缺口悬臂梁冲击  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 23℃  | 
			
				 880  | 
			
				 J/m  | 
			
				 ASTM D4812  | 
		
| 
				 23℃6  | 
			
				 53  | 
			
				 kJ/m²  | 
			
				 ISO 180/1U  | 
		
| 
				 装有测量仪表的落镖冲击  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 23℃,Total Energy  | 
			
				 11.3  | 
			
				 J  | 
			
				 ASTM D3763  | 
		
| 
				 --  | 
			
				 2.60  | 
			
				 J  | 
			
				 ISO 6603-2  | 
		
| 
				 热性能  | 
			
				 额定值  | 
			
				 单位制  | 
			
				 测试方法  | 
		
| 
				 热变形温度  | 
			
				 | 
			
				 | 
			
				 | 
		
| 
				 0.45 MPa,未退火,64.0 mm 跨距7  | 
			
				 214  | 
			
				 ℃  | 
			
				 ISO 75-2/Bf  | 
		
| 
				 1.8 MPa,未退火,3.20 mm  | 
			
				 201  | 
			
				 ℃  | 
			
				 ASTM D648  | 
		
| 
				 1.8 MPa,未退火,64.0 mm 跨距7  | 
			
				 191  | 
			
				 ℃  | 
			
				 ISO 75-2/Af  | 
		
| 
				 线形膨胀系数  | 
			
				 | 
			
				 | 
			
				 ASTM D696  | 
		
| 
				 流动:-30 到 30℃  | 
			
				 0.000044  | 
			
				 cm/cm/℃  | 
		|
| 
				 横向:-30 到 30℃  | 
			
				 0.00014  | 
			
				 cm/cm/℃  | 
		|
| 
				 注射  | 
			
				 额定值  | 
			
				 单位制  | 
		|
| 
				 干燥温度  | 
			
				 82.2  | 
			
				 ℃  | 
		|
| 
				 干燥时间  | 
			
				 4.0  | 
			
				 hr  | 
		|
| 
				 建议的最大水分含量  | 
			
				 0.15 到 0.25  | 
			
				 %  | 
		|
| 
				 螺筒后部温度  | 
			
				 249 到 260  | 
			
				 ℃  | 
		|
| 
				 螺筒中部温度  | 
			
				 266 到 277  | 
			
				 ℃  | 
		|
| 
				 螺筒前部温度  | 
			
				 277 到 288  | 
			
				 ℃  | 
		|
| 
				 加工(熔体)温度  | 
			
				 266 到 277  | 
			
				 ℃  | 
		|
| 
				 模具温度  | 
			
				 82.2 到 93.3  | 
			
				 ℃  | 
		|
| 
				 背压  | 
			
				 0.344 到 0.689  | 
			
				 MPa  | 
		|
| 
				 螺杆转速  | 
			
				 30 到 60  | 
			
				 rpm  | 
		|