POM WR140LG 抗紫外线,耐气候,光泽低

POM WR140LG 抗紫外线,耐气候,光泽低

Ticona HOSTAFORM POM WR140LG 是一款含有紫外线稳定剂的聚甲醛(POM)共聚物. 特点:光泽低,抗紫外线性能良好,良好的流动性,耐气候影响性能良好.
0.00
0.00
  
Ticona HOSTAFORM POM WR140LG 是一款含有紫外线稳定剂的聚甲醛(POM)共聚物. 特点:光泽低,抗紫外线性能良好,良好的流动性,耐气候影响性能良好.

HOSTAFORM® WR140LG CD34682 BLACK

 

HOSTAFORM WR140LG | POM | UV Resistant

 

Description

Hostaform® acetal copolymer grade WR140LG Black is a specialty weatherable grade of acetal copolymer formulated to provide good flow with a low gloss finish and a UV stability necessary for exterior automotive applications.

 

Other Processing

Injection Molding

Standard reciprocating screw injection molding machines with a high compression screw (minimum 3:1 and preferably 4:1) and low back pressure (0.35 Mpa/50 PSI) are favored. Using a low compression screw (I.E. general purpose 2:1 compression ratio) can result in unmelted particles and poor melt homogeneity. Using a high back pressure to make up for a low compression ratio may lead to excessive shear heating and deterioration of the material.

 

Melt Temperature: Preferred range 182-199 (360-390). Melt temperature should never exceed 230 (450).Mold Surface Temperature: Preferred range 82-93 (180-200) especially with wall thickness less than 1.5 mm (0.060 in.). May require mold temperature as high as 120 (250) to reproduce mold surface or to assure minimal molded in stress. Wall thickness greater than 3mm (1/8 in.) may use a cooler (65/150) mold surface temperature and wall thickness over 6mm (1/4 in.) may use a cold mold surface down to 25 (80). In general, mold surface temperatures lower than 82 (180) may hinder weld line formation and produce a hazy surface or a surface with flow lines, pits and other included defects that can hinder part performance.

 

ISO Data

Mechanical properties

Value

Unit

Test Standard

Phys

Density

1330

kg/m³

ISO 1183

Melt volume rate (MVR)

13

cm³/10min

ISO 1133

MVR test temperature

190

ISO 1133

MVR test load

2.16

kg

ISO 1133

Mold shrinkage - parallel

1.6

%

ISO 294-4

Mold shrinkage - normal

1.5

%

ISO 294-4

Mech

Mechanical properties

Value

Unit

Test Standard

Tensile modulus (1mm/min)

1800

MPa

ISO 527-2/1A

Tensile stress at yield (50mm/min)

41

MPa

ISO 527-2/1A

Tensile strain at yield (50mm/min)

10

%

ISO 527-2/1A

Flexural modulus (23)

1850

MPa

ISO 178

Charpy notched impact strength @ 23

3.6

kJ/m²

ISO 179/1eA

Charpy notched impact strength @ -30

3.6

kJ/m²

ISO 179/1eA

Therm

Thermal properties

Value

Unit

Test Standard

Melting temperature (10/min)

165

ISO 11357-1,-2,-3

DTUL @ 1.8 MPa

80

ISO 75-1/-2

Coeff.of linear therm. expansion (parallel)

1.3

E-4/

ISO 11359-2

Coeff.of linear therm. expansion (normal)

1.3

E-4/

ISO 11359-2

SpecProd

Test specimen production

Value

Unit

Test Standard

Processing conditions acc. ISO

9988-2

-

Internal

 

Processing

Pre Drying

Predrying is required before processing to ensure a low gloss finish. Use slow injection speed until material passes through gate, then increase.

 

Drying time (h)3

Drying temperature ()105 - 110

 

 